| Standards | GB/T 5213 | EN 10130 | JIS G3141 | DIN 1623-1 | |
| Grade | DC01 | DC01 | SPCC | St12 | |
| DC03 | DC03 | SPCD | St13 | ||
| DC04 | DC04 | SPCE | St14 | ||
| DC05 | DC05 | SPCF | - | ||
| DC06/DC07 | DC06/DC07 | SPCG | - | ||
| Mechanical Properties | |||||
| Grade | TensiIe test | ||||
| ReL(MPa) | Rm(MPa) | A80 (%) | r 90e | n 90e | |
| DC01 | 130~260 | ≥270 | ≥28 | - | - |
| DC03 | 120~240 | ≥270 | ≥34 | ≥1.3 | - |
| DC04 | 120~210 | ≥270 | ≥38 | ≥1.6 | ≥0.18 |
| DC05 | 110~190 | ≥270 | ≥40 | ≥1.9 | ≥0.20 |
| DC06 | 100~180 | ≥260 | ≥41 | ≥2.1 | ≥0.22 |
| DC07 | 100~160 | ≥250 | ≥44 | ≥2.5 | ≥0.23 |
| Tensile Strain Trace | |||||
| Grade | Tensile Strain Trace | ||||
| DC01 | It is guaranteed that no tension strain trace occurs on steel sheets and coils at theiapplication within 3 months after they are produced and in case of room temperature storage. |
||||
| DC03 | It is guaranteed that no tensile strain trace occurs on steel sheets and coils at theirapplication within 6 months after they are produced and in case of room temperaturestorage. | ||||
| DC04 | It is guaranteed that no tensile strain trace occurs on steel sheets and coils at theirapplication within 6 months after they are produced and in case of room temperaturestorage. | ||||
| DC05 | It is guaranteed that no tensile strain trace occurs on steel sheets and coils at theirapplication within 6 months after they are produced and in case of room temperaturestorage. | ||||
| DC06/DC07 | It is guaranteed that no tensile strain trace occurs on steel sheets and coils at theirapplication in case of room temperature storage. | ||||